News
What reason impact offset printing products?
1.Temperature and humidity of the environment. The environmental temperature is too low, the humidity
is too big can make the ink drying slowly.
2.The nature of the ink. In general, organic pigments inorganic pigments prepared ink is slow drying, thin
the binders than thick binders slow drying, the oil content of more than oil was less ink dried slowly.
3.The diluent and withdrawal Adhesives. The thinner and withdrawal viscosity to inhibit the dry nature of
the oil, plus heavy volume should be appropriate.
4.The nature and structure of the paper. Paper acidic, then blot dry slowly. Rough paper surface, loose
structure, permeability, facilities viscosity small will promote blot dry, and vice versa, then blot dry slowly.
5.PH value of the wetting liquid. Wetting fluid in hydrogen ion concentration, it will occur with the drying
oil in the metal substitution reaction, thereby suppressing drying of the ink on the paper surface.
6.The layout of water. In the printing process, if the layout is too large, not only makes the paper does
not absorb excessive moisture extending bulging, and will form an oil in water type emulsion ink, thus
affecting blot drying.
7.Desiccant plus let. Desiccant plus put too much, so coarse ink qualitative change, plate dirty Paste,
outlets expand deformation, with wool on barbed imprinted difficult to dry.sublimation offset ink,sublimation
offset transfer ink,sublimation offset printing ink
8.Sheets stacked too high. Large sheets of smooth paper, paper chop stacked too high, the air is difficult to
contact with printing ink, is bound to blot dry slowly.